Opening the kiln is the best moment of the week in a pottery studio, and occasionally the worst. A crack can feel like bad luck, but most cracks have a cause you can see once you know where to look.
Uneven thickness
Clay shrinks as it dries and again in the kiln. When one part of a pot is much thicker than another, the two parts shrink at different speeds and the clay tears where they meet. The most common place is where the wall joins a heavy base.
Trimming the foot carefully, and checking the base thickness with a needle tool, prevents most of these cracks.
Drying too fast
Rims and handles dry faster than the body of a pot. If they shrink while the rest is still soft, you get S-shaped cracks in the base or a handle that pulls away. In the dry Taos air this happens quickly.
Cover new work loosely with plastic and let it dry slowly for several days. Our studio has a damp cupboard for pieces that need extra time.
Trapped air and water
Air pockets left from poor wedging can expand in the kiln and blow out a section of the wall. Pieces that are not fully dry can crack or burst when the water turns to steam. We only load bisque firings with bone-dry work, and our teachers check every shelf before it goes in.
Joins that were not scored
Handles, lids and handbuilt slabs must be scored and joined with slip. Skipping this step leaves a seam that opens as the clay shrinks. Score both surfaces, add slip, press firmly and smooth the join. When a crack does appear, bring the piece to your teacher. Working out why it cracked is one of the fastest ways to get better at clay.